Bonding of steel structure enclosure materials

Solution

High-foaming DP heat-curing polyurethane spray glue series


SY8422D

Proportion100:40/30
Viscosity(25℃)mP-as5000-8000
Foaming rate600~800%
Departure time25-40s
Opening hours80-110s
Cure speed3.5min(45℃)

SY8422M1

Proportion100:40/30
Viscosity (25℃)mP-a57000~9000
Foaming rate600-800%
Departure time25-30s
Opening hours80-100s
Cure speed4.5min(45℃)

SY8422D1

Proportion100:40/30
Viscosity(25℃)mP-as3000~6000
Foaming rate600~800%
Departure time1.5~2min
Opening hours4~6min
Cure speed3.5min(45℃)

Special spray glue for bonding cement fiber cloth to rock wool

SY8422X5

Proportion100:50
Viscosity (25℃) mP·as2000-4000
Foaming rate800~1000%
Departure time25-40s
Opening hours80-100s
Cure speed3.5min(45℃)